| 油气田领域膨胀橡胶的膨胀性能研究 |
| Study on Swelling Properties of Swellable Rubber in Oil and Gas Fields |
| |
| DOI: |
| 中文关键词: 膨胀橡胶 遇油膨胀 遇水膨胀 膨胀性能 油气田 |
| 英文关键词: swellable rubber oil swelling water swelling swelling property oil and gas fields |
| 基金项目: |
| 中图分类号:TQ336.4+6 |
|
| 摘要点击次数: 2700 |
| 全文下载次数: 835 |
| 中文摘要: |
| 进行了油气田领域遇油膨胀橡胶[三元乙丙橡胶(EPDM)]和遇水膨胀橡胶[氢化丁腈橡胶(HNBR)]膨胀性能的研究。结果表明:温度对EPDM遇油膨胀橡胶和HNBR遇水膨胀橡胶的膨胀性能影响很大,温度越高,膨胀橡胶的膨胀尺寸越大;氯化钠溶液的质量分数越大,HNBR遇水膨胀橡胶的膨胀性能越差。EPDM遇油膨胀橡胶可在室温~200 ℃使用,HNBR遇水膨胀橡胶可在70~200 ℃使用,HNBR遇水膨胀橡胶在氯化钠溶液质量分数0.2以上仍可使用。 |
| 英文摘要: |
| In this work,the swelling properties of oil-swellable ethylene propylene diene monomer rubber(EPDM) and water-swellable hydrogenated nitrile butadiene rubber(HNBR) used in oil and gas fields were studied.The results showed that temperature greatly affected the swelling properties of the oil-swellable EPDM and water-swellable HNBR,and when the temperature increased,the swelling ratio increased.It was found that when the mass fraction of sodium chloride solution increased,the swelling performance of the water-swellable HNBR decreased.The oil-swellable EPDM could be used in the temperature range from room temperature to 200 ℃,while the water-swellable HNBR could be used from 70 to 200 ℃.The water-swellable HNBR could be used in the sodium chloride solution having a mass fraction above 0.2. |
|
|