李群,王志远.星形接枝溴化丁基橡胶在轮胎气密层中的应用[J].轮胎工业,2019,39(7):0414-0417 |
 二维码(扫一下试试看!) |
星形接枝溴化丁基橡胶在轮胎气密层中的应用 |
Application of Star Grafted Brominated Butyl Rubber in Inner-Liner of Tire |
投稿时间:2018-08-04 修订日期:2018-08-04 |
DOI:10.12135/j.issn.1006-8171.2019.07.0414 |
中文关键词: 溴化丁基橡胶 星形接枝 焦烧时间 收缩率 |
英文关键词: BIIR star grafted scorching time shrinkage |
基金项目: |
中图分类号: |
|
摘要点击次数: 1199 |
全文下载次数: 558 |
中文摘要: |
对比研究星形接枝溴化丁基橡胶(BIIR 6222)与通用溴化丁基橡胶(BIIR 2222)在轮胎气密层中的应用性能。结果表明:与BIIR 2222相比,BIIR 6222具有焦烧时间长、加工能耗低、压延尺寸收缩率低等优点,物理性能和气密性相当。 |
英文摘要: |
The application of star grafted brominated butyl rubber(BIIR 6222)and general brominated butyl rubber(BIIR 2222)in inner-liner of tire was compared and investigated.The results showed that,compared with BIIR 2222,BIIR 6222 had the advantages of long scorching time,low energy consumption and low shrinkage of calendering dimension.Its physical properties and air tightness were consistent with BIIR 2222. |
|