黄凯,黄黔.半钢子午线轮胎胎侧胶配方的改进[J].轮胎工业,2007,(11):676-678 |
 二维码(扫一下试试看!) |
半钢子午线轮胎胎侧胶配方的改进 |
Modification of sidewall formula of PCR tire |
|
DOI: |
中文关键词: 半钢子午线轮胎 胎侧胶 生热 高速耐久性能 |
英文关键词: PCR tire sidewall heat build-up high speed endurance performance |
基金项目: |
中图分类号:U463.341+.6 |
|
摘要点击次数: 1402 |
全文下载次数: 11 |
中文摘要: |
对半钢子午线轮胎胎侧胶配方进行改进,以提高轮胎的高速耐久性能。结果表明,通过适当增大硫黄和促进剂用量,胎侧胶的硫化速度加快、定伸应力和耐屈挠性能提高、生热降低,其它性能变化不大,成品轮胎的高速耐久性能显著改善。 |
英文摘要: |
The sidewall formula of PCR tire was modified to improve the high speed endurance performanceThe test results showed that,by increasing the additional level of sulfur and accelerator,the curing rate of sidewall compound increased,the modulus and the flexing resistance improved,the heat build up decreased,and other properties changed little.The high speed endurance performance of finished tire was improved significantly. |
|