文章摘要
贾明.NR内胎配方的优化设计[J].轮胎工业,2006,(11):669-671 本文二维码信息
二维码(扫一下试试看!)
NR内胎配方的优化设计
Optimization of NR inner tube formulation
  
DOI:
中文关键词: SBR  NR  内胎  粘合增进剂  材料成本
英文关键词: SBR  NR  inner tube  adhesion promoter
基金项目:
中图分类号:TQ332.6;TQ333.1;TQ336.12
作者单位
贾明 山东泰山轮胎有限公司 
摘要点击次数: 969
全文下载次数: 645
中文摘要:
      对NR内胎配方进行优化设计,通过采取调整硫化体系、增大粘合增进剂用量、严格控制生产工艺等措施,将内胎配方中SBR用量由40份增大到50份。试验表明,试验配方胶料工艺性能稳定,相应成品内胎各项性能均达到或超过国家标准要求,配方成本降低,具有显著的经济效益。
英文摘要:
      The NR inner tube formulation was optimized by modifying curing system,increasing addition level of adhesion promoter and strictly controlling manufacturing technology to increase the addition level of SBR in inner tube formula from 40 phr to 50 phr.The test results showed that the optimized compound featured stable processibility and lower cost,and the quality of finished inner tube met the requirements of relative national standard.
Author NameAffiliation
JIA Ming Shandong Taishan Tire Co.Ltd 